Kiln Formed Glass

Friday, December 21, 2012

12" Serving platter!
Pot melt flanked with strip cutting!

The latest from the kiln!
This piece required 12 kiln firings for a total of 102 hours in the kiln. It weighs 48 oz.
Posted by GlassWright at 12:16 PM No comments:
Email ThisBlogThis!Share to XShare to FacebookShare to Pinterest

Wednesday, December 12, 2012


Yellow River fused glass dish!

Posted by GlassWright at 8:41 AM No comments:
Email ThisBlogThis!Share to XShare to FacebookShare to Pinterest